Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 2.95 g/micron | 75.0 g/mil | ASTM D1922 |
ExxonMobil LD 071.MU Blown Film Resin
(discontinued **) LD 071 series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, toughness, burn-through re.. |