Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 8.30 g/micron | 211 g/mil | ASTM D1922 |
Braskem ES 300 HDPE Blown Film Extrusion Polyethylene
(discontinued **) 38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Grocery and T-shirt bags; merchandise bags; frozen-food bags; high-strength films. Informa.. |
|||
Elmendorf Tear Strength, TD | 8.30 g/micron | 211 g/mil | |
Dow LDPE 640I Low Density Polyethylene, Liner Film Grade DOW LDPE 640I resin is a barefoot general purpose liner film resin for thin gauge applications requiring good drawdown and excellent toughness. This material complies with U.S.FDA regulation 21 CFR .. |
|||
Elmendorf Tear Strength, TD | 8.30 g/micron | 211 g/mil | |
Dow Primacor® 1420 Ethylene Acrylic Acid (EAA) Film properties below based on a film thickness of 60 µm. Data provided by Dow Chemical. |
|||
Elmendorf Tear Strength, TD | 8.30 g/micron | 211 g/mil | ASTM D-1922 |
Bapolene® 200F Polyethylene, Film Grade Bapolene LD200F is a general purpose low density polyethylene for blown film extrusion applications. It contains medium levels of slip/antiblock additives. This product meets FDA standards for foo.. |