Polymer Property : Elmendorf Tear Strength, TD = 24.6 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 24.6 g/micron
625 g/mil
ASTM D1922
ExxonMobil Exceed™ 3518 GA Premium Cast Film Resin  (discontinued **)
Exceed 3518 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3518 resins have outstanding tensile properties and impact and puncture toughness. ..
Elmendorf Tear Strength, TD 24.6 g/micron
625 g/mil
ASTM D1922
Dow FLEXOMER™ ETS-9064 NT 7, 0.8 mil Very Low Density Polyethylene (VLDPE) Resin
FLEXOMER™ ETS-9064 NT 7 is intended for use in single of multi-layer blown-film constructions or thick sheets. Films extruded from ETS-9064 NT 7 have a high tear strength, high impact strength, an..
Elmendorf Tear Strength, TD 24.6 g/micron
625 g/mil
ASTM D1922
ExxonMobil Escorene® LL-3201 LLDPE/Hexene Premium High Strength 1.2 mil Film, Stiff  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.An LLDPE hexene copolymer film resin. Films made from this resin have outstanding tensile, stiffness and toughness properties. These superior prope..
Elmendorf Tear Strength, TD 24.6 g/micron
625 g/mil
ASTM D1922
ExxonMobil Exceed™ 3518 CB Premium Cast Film Resin
Exceed 3518 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3518 resins have outstanding tensile properties and impact and puncture toughness. ..
Elmendorf Tear Strength, TD 24.6 g/micron
625 g/mil
ASTM D1922
ExxonMobil Exceed™ 3518 PA Premium Cast Film Resin
Exceed 3518 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3518 resins have outstanding tensile properties and impact and puncture toughness. ..