Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 3.70 g/micron
94.0 g/mil
ASTM D1922
Eastman E6838-795F Polyethylene  (discontinued **)
E6838-795F is a low density formulation with no slip or antiblock level. It is suggested for film applications that require a good balance of properties such as converter film for industrial packag..
Elmendorf Tear Strength, TD 3.70 g/micron
94.0 g/mil
ASTM D1922
Eastman E6838-796F Polyethylene  (discontinued **)
E6838-796F is a low density formulation with no slip or antiblock. It is suggested for film applications requiring a good balance of properties, such as converter film for industrial packaging, gen..
Elmendorf Tear Strength, TD 3.70 g/micron
94.0 g/mil
ASTM D1922
Eastman E6838-964F Polyethylene  (discontinued **)
E6838-964F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require a good balance of physical and optical properties.List of Applicati..
Elmendorf Tear Strength, TD 3.70 - 5.24 g/micron
94.0 - 133 g/mil
Average value: 4.36 g/micron Grade Count:4
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade". Each property range of values reported..
Elmendorf Tear Strength, TD 3.70 g/micron
94.0 g/mil
DuPont™ Surlyn® 1652-1 Zinc Ionomer Resin for Blown/Cast Film and Extrusion Coating  (discontinued **)
Surlyn® 1652-1 is an ionomer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylen..
Elmendorf Tear Strength, TD 3.70 g/micron
94.0 g/mil
50 µm (2 mil) film; ASTM D1922
DuPont Elvax® 3170 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film
18 wt% Vinyl Acetate.Elvax® 3170 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins..
Elmendorf Tear Strength, TD 3.70 g/micron
94.0 g/mil
ISO 6383-2
Total EVA 1010 VN 3 Ethylene Vinyl Acetate Copolymer - Blown Film
EVA 1010 VN 3 is made by a high pressure tubular process. Grade for films with high transparency and high mechanical properties. Contains an antioxidant.Application examples: Stretch film, food pa..
Elmendorf Tear Strength, TD 3.70 g/micron
94.0 g/mil
ASTM D1922
Eastman E6838-963F Polyethylene  (discontinued **)
E6838-963F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require a good balance of physical and optical properties.List of Applicati..