Material Notes:
E6838-964F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require a good balance of physical and optical properties.List of Applications: Food-contact applicationsFood packagingE6838-964F meets the requirements of FDA regulations at 21 CFR 177.1520(c)(2.2) and may be used as a component of packages used for holding food during cooking. However, the polymer thickness in the form in which it contacts food shall not exceed 0.005 inches and contact is limited to non-alcoholic food because of a regulatory limitation for an adjuvant substance in this formulation.Information supplied by the manufacturer.Information from manufacturer data sheet.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line.
Physical Properties Metric English Comments
Density 0.921 g/cc
0.0333 lb/in³
ASTM D4883
Thickness 38.0 microns
1.50 mil
Melt Flow 1.3 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.3 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 30.0 MPa
4350 psi
ASTM D882
Film Tensile Strength at Yield, TD 11.0 MPa
1600 psi
ASTM D882
Film Elongation at Break, MD 200 %
200 %
ASTM D882
Film Elongation at Break, TD 750 %
750 %
ASTM D882
Secant Modulus, MD 0.193 GPa
28.0 ksi
1% Secant; ASTM D882
Secant Modulus, TD 0.240 GPa
34.8 ksi
1% Secant; ASTM D882
Coefficient of Friction 0.60
0.60
ASTM D1894
Elmendorf Tear Strength MD 400 g
400 g
Elmendorf Tear Strength TD 140 g
140 g
Elmendorf Tear Strength, MD 10.5 g/micron
267 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 3.70 g/micron
94.0 g/mil
ASTM D1922
Dart Drop 3.20 g/micron
81.3 g/mil
ASTM D1709A
Film Tensile Strength at Break, MD 31.0 MPa
4500 psi
ASTM D882
Film Tensile Strength at Break, TD 21.0 MPa
3050 psi
ASTM D882
Thermal Properties Metric English Comments
Vicat Softening Point 95.0 °C
203 °F
ASTM D1525
Optical Properties Metric English Comments
Haze 6.0 %
6.0 %
ASTM D1003
Gloss 70 %
70 %
at 45°; ASTM D2457
Transmission, Visible 95 %
95 %
ASTM D1746
Descriptive Properties Value Comments
Process Film
Users viewing this material also viewed the following: