Polymer Property : Elmendorf Tear Strength, TD = 465.89 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 18.342 g/micron
465.89 g/mil
ISO 6383-2
Polimeri Europa Eraclene® FB 506 Hexene Copolymer High Density Polyethylene - Blown Film Extrusion
Eraclene FB 506 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.Its broad molecular weight distribution and density successfully c..
Elmendorf Tear Strength, TD 18.342 g/micron
465.89 g/mil
ISO 6383-2
Polimeri Europa Flexirene® FF 25 Butene Copolymer Linear Low Density Polyethylene
Flexirene FF 25 is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Flexirene FF 25 is characterized by a high elongational viscosi..
Elmendorf Tear Strength, TD 18.342 g/micron
465.89 g/mil
ISO 6383-2
Polimeri Europa Flexirene® FG 30 Butene Copolymer Linear Low Density Polyethylene
Flexirene FG 30 is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Films manufactured with Flexirene FG 30 are characterized by an..
Elmendorf Tear Strength, TD 18.342 g/micron
465.89 g/mil
ISO 6383-2
Polimeri Europa Flexirene® FG 30 U Butene Copolymer Linear Low Density Polyethylene
Flexirene FG 30 U is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Films manufactured with Flexirene FG 30 U are characterized b..
Elmendorf Tear Strength, TD 18.342 g/micron
465.89 g/mil
ISO 6383-2
Polimeri Europa Clearflex® CM 406 Hexene Copolymer Linear Low Density Polyethylene
Clearflex CM 406 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for cast film extrusion.Films manufactured with Clearflex CM 406 are characterized by h..