Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa Flexirene® FF 25 Butene Copolymer Linear Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE)/Butene, Film
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Flexirene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Flexirene® FF 25 Butene Copolymer Linear Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flexirene FF 25 is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Flexirene FF 25 is characterized by a high elongational viscosity leading to a good bubble stability during extrusion.Main Applications: Flexirene FF 25 is recommended for the production of agriculture film, heavy duty bags, in blend or coextrusion with LDPE.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ISO 1183
Thickness 15.0 - 50.0 microns
0.591 - 1.97 mil
Recommended
Melt Flow 0.75 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.75 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 11.0 MPa
1600 psi
ISO 527-3
Film Tensile Strength at Yield, TD 11.0 MPa
1600 psi
ISO 527-3
Film Elongation at Break, MD 580 %
580 %
ISO 527-3
Film Elongation at Break, TD 800 %
800 %
ISO 527-3
Coefficient of Friction, Dynamic >= 0.50
>= 0.50
ISO 8295
Elmendorf Tear Strength, MD 2.5475 g/micron
64.706 g/mil
ISO 6383-2
Elmendorf Tear Strength, TD 18.342 g/micron
465.89 g/mil
ISO 6383-2
Dart Drop Test 100 g
0.221 lb
F50; ISO 7765-1
Film Tensile Strength at Break, MD 45.0 MPa
6530 psi
ISO 527-3
Film Tensile Strength at Break, TD 32.0 MPa
4640 psi
ISO 527-3
1% Secant Modulus, MD 200 MPa
29000 psi
ISO 527-3
1% Secant Modulus, TD 210 MPa
30500 psi
ISO 527-3
Thermal Properties Metric English Comments
Melting Point 120 °C
248 °F
Internal method
Vicat Softening Point 98.0 °C

@Load 1.00 kg
208 °F

@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D746
Optical Properties Metric English Comments
Haze 12 %
12 %
ISO 14782
Gloss 55 %
55 %
45°; ASTM D2457
Users viewing this material also viewed the following: