Polymer Property : Elmendorf Tear Strength, TD = 5.40 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 5.40 g/micron
137 g/mil
ASTM D1922
Eastman E6838-923F Polyethylene  (discontinued **)
E6838-923F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require heat-sealing treated-to-treated film surfaces and where good clarit..
Elmendorf Tear Strength, TD 5.40 g/micron
137 g/mil
ASTM D1922
Petroquimica Triunfo Trithene® TS 8064 LDPE - Packaging Film
The Trithene TS 8064 resin is a low-density polyethylene (LDPE) with a medium molecular weight an excellent processability. Furthermore, this product has good mechanical properties, average transpar..
Elmendorf Tear Strength, TD 5.40 g/micron
137 g/mil
ASTM-D1922
Braskem TN2005 EVA General Film Copolymer
TN2005 is an Ethylene-Vinyl Acetate (EVA) copolymer with high molecular weight, excellent mechanical properties, transparency, high gloss, and easy processing. Additionally, TN2005 has flexibility e..