Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 5.90 g/micron | 150 g/mil | ASTM D 1922 |
NOVA Chemicals Surpass® HPs167-AB Homopolymer sHDPE Film Resin HPs167-AB complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Che.. |
|||
Elmendorf Tear Strength, TD | 5.90 g/micron | 150 g/mil | ASTM D1922 |
Petroquimica Triunfo Tritheva® TN 8093 EVA Copolymer The Tritheva TN 8093 resin is a fractional MI copolymer of Ethylene-Vinyl Acetate (EVA), developed to meet the multi-layer and blending film applications where are required high strength, with high .. |