Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dart Drop Test = 0.187 lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop Test 85.0 g
0.187 lb
ASTM D1709
SABIC 218 Series Linear Low Density Polyethylene for Blown Film
Product Description: 218 series resins are Linear Low Density Polyethylene grades suitable for general purpose packaging. They are easy to process giving good tensile properties, impact strength a..
Dart Drop Test 85.0 g
0.187 lb
ASTM D1709
SABIC 726 Series Linear Low Density Polyethylene for Blown Film
Product Description: 726 series resins are fractional index Linear Low Density Polyethylene grades suitable for blown film applications. Films produced using these resins give a relatively higher ..
Dart Drop Test 85.0 g
0.187 lb
F50; ASTM D-1709
ExxonMobil Escorene® LL-1042 LLDPE Packaging Film Resin, Clarity  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.An LLDPE blown clarity film resin. Films made from LL-1042 have very good tensile properties and toughness in addition to good clarity The good st..
Dart Drop Test 85.0 g
0.187 lb
F50; ASTM D-1709
ExxonMobil Escorene® LL-3023 LLDPE/Hexene Premium Cast Stretch Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3023 have outstanding tensile properties as well as stiffness and toughness.Applicatio..
Dart Drop Test 85.0 g
0.187 lb
F50; ASTM D-1709
ExxonMobil Escorene® LD-102 LDPE Drawdown Resin, 1.25 mil Film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A homopolymer, good clarity, laundry and dry cleaning film resin capable of providing a tough film in very thin gauges.Applications: Dry cleaning es..
Dart Drop Test 85.0 - 100 g
0.187 - 0.221 lb
ASTM D1709
Huntsman PE 1017 Film Extrusion Polyethylene  (discontinued **)
Homopolymer, Drug Master File listed product, and FDA compliant.Features: Good impact strength, good machinability, heat seal and foaming characteristicsApplications: Film Extrusion: industrial line..
Dart Drop Test 85.0 - 700 g
0.187 - 1.54 lb
Average value: 290 g Grade Count:5
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade". Each property range of values reported..
Dart Drop Test 85.0 g
0.187 lb
ASTM D1709
Total HDPE 6480 High Density Polyethylene, Clarity Cast Film Resin
Polyethylene: Clarity High Density Cast Film ResinCharacteristics:High stiffnessHigh clarityExcellent surface glossHigh tensile strengthGood barrier propertiesLow gel contentApplications:OverwrapFo..