Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 365 g | 0.805 lb | ASTM D1709 |
Arkema Group OREVAC® 9314 EVA Terpolymer OREVAC® is a range of ethylene-vinyl acetate copolymers modified by adjunction of polar groups which, when molten, have excellent adhesive properties to various substrates. They are supplied as fre.. |
|||
Dart Drop Test | 365 g | 0.805 lb | 50 microns film |
Arkema Group Orevac® 9314 Film EVA-MAH Terpolymer EVA Terpolymers based Main Application: Blown film coextrusionInformation provided by Arkema Group |