Mechanical Properties Metric English Comments
Dart Drop Test 390 g
0.860 lb
F50; ISO 7765-1
Polimeri Europa Clearflex® H&T FGH 196 Hexene Copolymer Linear Low Density Polyethylene
Clearflex H&T FGH 196 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films obtained from Clearflex H&T FGH ..
Dart Drop Test 390 g
0.860 lb
ASTM D1709
Solvay Specialty Polymers Ajedium™ Films -- Veradel® PES 201 NT Polyethersulfone (PESU)
Veradel® PES 201 NT polyethersulfone is a tough, high-strength thermoplastics that are suitable for continuous use up to 356°F (180°C). Veradel® film is resistant to oxidation and hydrol..
Dart Drop Test 390 g
0.860 lb
ASTM D1709
Solvay Specialty Polymers Ajediumâ„¢ KT-820 Polyetheretherketone (PEEK)
KetaSpire® KT-820 PEEK film is thermoplastic film that is characterized by a distinct combination of properties, which include excellent wear resistance, best-in-class fatigue resistance, high pu..
Dart Drop Test 390 g
0.860 lb
D1709
Westlake EF528 18.5% Ethylene Vinyl Acetate Copolymer
Westlake ELEVATE™ EF528 is an ethylene vinyl acetate copolymer with 18.5% VA. EF528 is designed for blown and cast films requiring excellent optics and low heat seal initiation. High melt strength ..
Dart Drop Test 390 g
0.860 lb
ASTM D1709
Westlake Elevate™ DA528AA 18.5% Ethylene Vinyl Acetate Copolymer
Westlake ELEVATE™ DA528 is an ethylene vinyl acetate copolymer with 18.5% VA. DA528 is designed for blown and cast films requiring excellent optics and low heat seal initiation. High melt strength..
Dart Drop Test 390 g
0.860 lb
ASTM D1709
Westlake Elevate™ DA528AA Ethylene Vinyl Acetate Copolymer
Developmental ProductDescription: Westlake ELEVATE™ DA528 is an ethylene vinyl acetate copolymer with 18.5% VA. DA528 is designed for blown and cast films requiring excellent optics and low heat s..
Dart Drop Test 390 g
0.860 lb
ASTM D1709A
ExxonMobil Escorene™ FL 00209 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: FL 00209 is a copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 270°C (518°F) may cause resin degradation. Machines should always b..
Dart Drop Test 390 g
0.860 lb
ASTM D1709A
Westlake EMAC® SP2261 23% Ethylene-Methyl Acrylate Copolymer
Westlake EMAC® SP2261 is a 23% EMA copolymer containing antiblock. This resin is designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal tempe..