Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 390 g | 0.860 lb | F50; ISO 7765-1 |
Polimeri Europa Clearflex® H&T FGH 196 Hexene Copolymer Linear Low Density Polyethylene Clearflex H&T FGH 196 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films obtained from Clearflex H&T FGH .. |
|||
Dart Drop Test | 390 g | 0.860 lb | ASTM D1709 |
Solvay Specialty Polymers Ajedium™ Films -- Veradel® PES 201 NT Polyethersulfone (PESU) Veradel® PES 201 NT polyethersulfone is a tough, high-strength thermoplastics that are suitable for continuous use up to 356°F (180°C). Veradel® film is resistant to oxidation and hydrol.. |
|||
Dart Drop Test | 390 g | 0.860 lb | ASTM D1709 |
Solvay Specialty Polymers Ajedium™ KT-820 Polyetheretherketone (PEEK) KetaSpire® KT-820 PEEK film is thermoplastic film that is characterized by a distinct combination of properties, which include excellent wear resistance, best-in-class fatigue resistance, high pu.. |
|||
Dart Drop Test | 390 g | 0.860 lb | D1709 |
Westlake EF528 18.5% Ethylene Vinyl Acetate Copolymer Westlake ELEVATE™ EF528 is an ethylene vinyl acetate copolymer with 18.5% VA. EF528 is designed for blown and cast films requiring excellent optics and low heat seal initiation. High melt strength .. |
|||
Dart Drop Test | 390 g | 0.860 lb | ASTM D1709 |
Westlake Elevate™ DA528AA 18.5% Ethylene Vinyl Acetate Copolymer Westlake ELEVATE™ DA528 is an ethylene vinyl acetate copolymer with 18.5% VA. DA528 is designed for blown and
cast films requiring excellent optics and low heat seal initiation. High melt strength.. |
|||
Dart Drop Test | 390 g | 0.860 lb | ASTM D1709 |
Westlake Elevate™ DA528AA Ethylene Vinyl Acetate Copolymer Developmental ProductDescription: Westlake ELEVATE™ DA528 is an ethylene vinyl acetate copolymer with 18.5% VA. DA528 is designed for blown and cast films requiring excellent optics and low heat s.. |
|||
Dart Drop Test | 390 g | 0.860 lb | ASTM D1709A |
ExxonMobil Escorene™ FL 00209 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00209 is a copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 270°C (518°F) may cause resin degradation. Machines should always b.. |
|||
Dart Drop Test | 390 g | 0.860 lb | ASTM D1709A |
Westlake EMAC® SP2261 23% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2261 is a 23% EMA copolymer containing antiblock. This resin is designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal tempe.. |