Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 145 g | 0.320 lb | F<sub>50</sub>; ASTM D1709A |
LyondellBasell Petrothene® GA501020 Linear Low Density Polyethylene ApplicationsPETROTHENE GA 501series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These resins have excellent .. |
|||
Dart Drop Test | 145 g | 0.320 lb | F<sub>50</sub>; ASTM D1709A |
LyondellBasell Petrothene® GA501021 Linear Low Density Polyethylene ApplicationsPETROTHENE GA 501series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These resins have excellent .. |
|||
Dart Drop Test | 145 g | 0.320 lb | F<sub>50</sub>; ASTM D1709A |
LyondellBasell Petrothene® GA501022 Linear Low Density Polyethylene ApplicationsPETROTHENE GA 501series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These resins have excellent .. |
|||
Dart Drop Test | 145 g | 0.320 lb | F<sub>50</sub>; ASTM D1709A |
LyondellBasell Petrothene® GA501023 Linear Low Density Polyethylene ApplicationsPETROTHENE GA 501series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These resins have excellent .. |
|||
Dart Drop Test | 145 g | 0.320 lb | F50; ASTM D-1709 |
ExxonMobil Escorene® LL-3201 LLDPE/Hexene Premium High Strength 1.2 mil Film, Stiff
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE hexene copolymer film resin. Films made from this resin have outstanding tensile, stiffness and toughness properties. These superior prope.. |