Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 320 g | 0.706 lb | F50; ISO 7765-1 |
Polimeri Europa Riblene® FC 39 Low Density Polyethylene - Blown Film Extrusion Riblene FC 39 is a high molecular weight low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FC 39 is characterized by a high melt strength leading to a good bubble stability.. |
|||
Dart Drop Test | 320 g | 0.706 lb | ASTM D 1709 |
Total Finathene® 1288 HDPE film
(discontinued **) Applications: Flat bottom bags, draw strings, coextruded merchandise bags, deli wrapInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plasti.. |
|||
Dart Drop Test | 320 g | 0.706 lb | ASTM D1709 |
LG Chemical SEETEC ST318 Linear Low Density Polyethylene, Blown Film Grade Features: Characteristics- Excellent puncture resistance, tear strength. Excellent sealing and optical properties. Comonomer: Octene-1. Additives- Medium slip agent, Medium antiblocking agentApplica.. |
|||
Dart Drop Test | 320 g | 0.706 lb | F<sub>50</sub>; ASTM D1709 |
LyondellBasell Petrothene® NA480145 Low Density Polyethylene ApplicationsPETROTHENE NA 480 is a series of low density/EVA copolymer resins designed for specialty films. NA 480 produces film with superior puncture resistance, Heat sealability, clarity and low.. |
|||
Dart Drop Test | 320 g | 0.706 lb | F<sub>50</sub>; ASTM D1709 |
LyondellBasell Petrothene® NA480177 Low Density Polyethylene ApplicationsPETROTHENE NA 480 is a series of low density/EVA copolymer resins designed for specialty films. NA 480 produces film with superior puncture resistance, Heat sealability, clarity and low.. |
|||
Dart Drop Test | 320 g | 0.706 lb | F<sub>50</sub>; ASTM D1709 |
LyondellBasell Petrothene® NA480178 Low Density Polyethylene ApplicationsPETROTHENE NA 480 is a series of low density/EVA copolymer resins designed for specialty films. NA 480 produces film with superior puncture resistance, Heat sealability, clarity and low.. |
|||
Dart Drop Test | 320 g | 0.706 lb | ISO 7765-1 |
Total PPR 6288 Random Copolymer Polypropylene, Cast Extrusion of Film Total Petrochemicals PPR 6288 is a random copolymer polypropylene with a melt flow index of 8 g/10 min for the cast extrusion of films with outstanding optical properties and easy heat weldability.P.. |
|||
Dart Drop Test | 320 g | 0.706 lb | ASTM D1709A |
ExxonMobil Escorene® LD 713.93 Blown Film Resin Escorene Ultra LD 713.93 is a 14.4 wt% vinyl acetate copolymer film resin. Film made from LD 713.93 exhibits very high impact strength, high clarity, and excellent heat sealability.Availability: Lat.. |
|||
Dart Drop Test | 320 g | 0.706 lb | ASTM D1709A |
ExxonMobil LDPE LD 165BW1 Low Density Polyethylene Resin (European Grade) Product Description: LD 165 series are LDPE grades, offering high strength combined with medium optical properties.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoTherm.. |
|||
Dart Drop Test | 320 g | 0.706 lb | ASTM D1709 |
ExxonMobil Pax-Plus™ 3201 Blown Film Resin Pax-Plus 3201 is a rubber modified high density polyethylene film resin that exhibits excellent impact strength and stress crack resistance. It is used primarily in film where its good tear resista.. |
|||
Dart Drop Test | 320 g | 0.706 lb | ASTM D1709 |
LG Chemical SEETEC SF318 Linear Low Density Polyethylene, Blown Film Grade Features: Characteristics- Good tensile & tear strength, High clarity, mechanical strength & sealing properties. Comonomer: Octene-1. Additives- Medium slip agent, Medium antiblocking agentApplicati.. |
|||
Dart Drop Test | 320 g | 0.706 lb | ASTM D1709 |
LG Chemical SEETEC SN318 Linear Low Density Polyethylene, Blown Film Grade Features: Characteristics- Good tensile & tear strength, High clarity, mechanical strength & sealing properties. Comonomer: Octene-1. Additives- Medium slip agent, Medium antiblocking agentApplicati.. |