Mechanical Properties Metric English Comments
Dart Drop Test 500 g
1.10 lb
ISO 7765-1
Borealis FT3200 Low Density Polyethylene
FT3200 is a Low Density Polyethylene for Film Extrusion. Applications heavy-duty bags, shrink film, construction films, and agricultural films. FT3200 contains no additives.Information provided by..
Dart Drop Test 500 g
1.10 lb
ISO 7765-1
Total EVA 1020 VN 5 Ethylene Vinyl Acetate Copolymer - Blown Film
EVA 1020 VN 5 is made by a high pressure tubular process. Grade for very flexible films with very high transparency and good mechanical properties. Contains an antioxidant.Application examples: Ch..
Dart Drop Test 500 g
1.10 lb
ASTM D1709
ExxonMobil Exceed™ 1012 MJ Metallocene Polyethylene Resin
Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymers. Films made from Exceed 1012 mVLDPE resin have outstanding cold temperature toughness, impact strength and p..
Dart Drop Test 500 g
1.10 lb
ASTM D1709
ExxonMobil Exceed™ 1012 MK Metallocene Polyethylene Resin
Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymers. Films made from Exceed 1012 mVLDPE resin have outstanding cold temperature toughness, impact strength and p..
Dart Drop Test 500 g
1.10 lb
Method A; ASTM D1709
Dow DOWLEX™ 2020G Linear Low Density Polyethylene
DOWLEX™ 2020G is perfect for high strength consumer trash bags/liners. This product can be used in other applications that require toughness and also offers great melt strength for high throughput..