ExxonMobil Exceed™ 1012 MK Metallocene Polyethylene Resin

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Exxon Chemical
Trade Name Exceed™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Exceed™ 1012 MK Metallocene Polyethylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymers. Films made from Exceed 1012 mVLDPE resin have outstanding cold temperature toughness, impact strength and puncture. These superior strength properties, along with excellent heat sealing and hot tack performance, make this a very versatile packaging film resin.Availability: Latin America, North America and South AmericaAdditive:Antiblock: 5000 ppmSlip: 1000 ppmProcessing Aid: YesThermal Stabilizer: YesApplications:Bag in BoxBarrier Food PackagingBlown FilmFood packagingForm Fill and Seal PackagingFreezer FilmHeavy Duty BagsIce BagsLamination FilmMultilayer Packaging Film Stand Up Pouches Information provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.912 g/cc
0.0329 lb/in³
ExxonMobil method
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Antiblock Level 5000 ppm
5000 ppm
Slip Level 1000 ppm
1000 ppm
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 6.89 MPa
1000 psi
ASTM D882
Film Tensile Strength at Yield, TD 7.58 MPa
1100 psi
ASTM D882
Film Elongation at Break, MD 460 %
460 %
ASTM D882
Film Elongation at Break, TD 580 %
580 %
ASTM D882
Puncture Energy 2.94 J
2.17 ft-lb
ExxonMobil Method
Elmendorf Tear Strength MD 210 g
210 g
ASTM D1922
Elmendorf Tear Strength TD 330 g
330 g
ASTM D1922
Dart Drop Test 500 g
1.10 lb
ASTM D1709
Film Tensile Strength at Break, MD 54.5 MPa
7900 psi
ASTM D882
Film Tensile Strength at Break, TD 48.3 MPa
7000 psi
ASTM D882
1% Secant Modulus, MD 117 MPa
17000 psi
ASTM D882
1% Secant Modulus, TD 131 MPa
19000 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point <= 242 °C
<= 468 °F
Peak Melting Point; ExxonMobil method
Optical Properties Metric English Comments
Haze 15 %
15 %
ASTM D1003
Gloss 45 %
45 %
45°; ASTM D2457
Descriptive Properties Value Comments
Puncture Force 10 lbf
ExxonMobil Method