Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 85.5 MPa
12400 psi
ASTM D882A
DuPont Teijin Films Melinex® 534 Polyester Film, 380 Gauge
Melinex® 534 is an opaque white film with superb handling properties and a unique glossy appearance. It is pre-treated on both surfaces to promote adhesion to aqueous based inks and coatings.Inform..