Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Film Tensile Strength at Break, TD = 14.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 14.0 MPa
2030 psi
ASTM D882
Petroquimica Triunfo Trithene® CX 7065 LDPE - Extrusion Coating
The Trithene® CX 7065 resin is a product developed especially to meet the segment of extrusion coating where the following properties are necessary: processing stability at high production rates, a..
Film Tensile Strength at Break, TD 14.0 MPa
2030 psi
ASTM D882
Westlake EMAC® SP2242 Specialty Copolymer  (discontinued **)
EMAC resins adhere to and are compatible with a wide range of materials including paper, polyolefins, oriented polyolefins, polyesters, ionomers, PVdC, unplasticized PVC and other polar polymers. Fo..
Film Tensile Strength at Break, TD 14.0 MPa
2030 psi
ASTM D882
Huntsman PE1058 Film Extrusion Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Exceptional draw down and processability, excellent strength, good heat sealability, and optics.Applications: Film extrusion: all thin film uses and especiall..
Film Tensile Strength at Break, TD 14.0 MPa
2030 psi
ASTM D882
Huntsman PE1068 Film Extrusion Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Exceptional draw down and processability even to 1/2 mil; excellent strength, good heat sealability, and good optical.FDA Notes: Conforms to FDA regulation 21..
Film Tensile Strength at Break, TD 14.0 MPa
2030 psi
ASTM D882
Huntsman PE5030 Extrusion Coating Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Good draw down, low neck-in, good heat sealability and adhesion, low smoking, and excellent printabilityApplications: Extrusion: coating grade and general coa..
Film Tensile Strength at Break, TD 14.0 MPa
2030 psi
ASTM D882
Huntsman PE5032 Extrusion Coating Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Excellent draw down, low neck-in, excellent heat sealability, good adhesion, low smoking, no edge weave, and excellent printability.Applications: Extrusion: c..
Film Tensile Strength at Break, TD 14.0 MPa
2030 psi
ASTM D822
Westlake EMAC® Plus SP1358 21.5% Ethylene-Methyl Acrylate Copolymer
Westlake EMAC® Plus SP1358 is a 21.5% EMA copolymer containing slip and antiblock. This resin is designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low..
Film Tensile Strength at Break, TD 14.0 MPa
2030 psi
ASTM D882
Huntsman Rexell® V3401 Blown Film Extrusion LLDPE  (discontinued **)
Ultra linear low density copolymer, cast film extrusion, FDA compliant.Features: Excellent processability, toughness, and optics with good sealing properties.Applications: Sealing layer in coextrude..
Copyright © lookpolymers.com All Rights Reserved