Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 15.2 MPa
2200 psi
ASTM D882
Westlake EF677 Low Density Polyethylene
Westlake EF677 is a high melt index LDPE resin suggested for garment films, or other applications requiring excellent drawdown. This material is also an excellent choice for PE foam applications.App..
Film Tensile Strength at Break, TD 15.2 MPa
2200 psi
ASTM D882
ExxonMobil Escorene™ LD 723.28 Cast Ethylene Vinyl Acetate Copolymer
Product Description: Escorene Ultra UL 723.28 is a high VA extrusion coating resin, which provides outstanding heat sealability and high clarity. LD 723.28 has a good balance of drawabilty and neck-..
Film Tensile Strength at Break, TD 15.2 MPa
2200 psi
ASTM D882
ExxonMobil LDPE LD 160AT Low Density Polyethylene Resin
Product Description: LD 160 series are LDPE grades, which offer good draw down and optical properties.Availability: Africa & Middle East, Asia Pacific, Latin America, North America and South America..
Film Tensile Strength at Break, TD 15.2 MPa
2200 psi
ASTM D882
Dow INTEGRAL™ 933 Tough Film for Lamination to Porous Substrates
INTEGRAL 933 Adhesive Film has a low melting, high flow adhesive layer that is useful for bonding to substrates such as polyurethane or polyethylene foam, or to non-woven textiles.Information provid..
Film Tensile Strength at Break, TD 15.2 MPa
2200 psi
Dow LDPE 526A Low Density Polyethylene, Blown Film Grade
DOW LDPE 526A resin is a general purpose blown film extrusion resin for use in medium duty liner film applications and other packaging applications. It contains medium levels of antiblock additive. ..
Film Tensile Strength at Break, TD 15.2 MPa
2200 psi
Dow LDPE 527A Low Density Polyethylene, Blown Film Grade
DOW LDPE 527A is a general purpose blown film extrusion resin for use in medium duty liner film applications and other packaging applications. It contains high levels of antiblock additive. This mat..
Film Tensile Strength at Break, TD 15.2 MPa
2200 psi
Dow LDPE 586A Low Density Polyethylene, Packaging Grade
DOW LDPE 586A resin is used for general purpose packaging applications. It contains medium levels of slip additive and low levels of antiblock additive. This material complies with U.S.FDA regulatio..
Film Tensile Strength at Break, TD 15.2 - 45.0 MPa
2200 - 6530 psi
Average value: 22.8 MPa Grade Count:13
Overview of materials for Low Density Polyethylene (LDPE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum ..