Polymer Property : Film Tensile Strength at Break, TD = 155 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 155 MPa
22500 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Label-Lyte™ 33LL247 OPP Film
Product Description: A super white opaque, high gloss, caviated BOPP film designed for use in reel-fed warp-around labeling applications where superior graphics are desired.Availability: Africa & Mi..
Film Tensile Strength at Break, TD 155 MPa
22500 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Label-Lyte™ 38LL247 OPP Film
Product Description: A super white opaque, high gloss, cavitated BOPP film designed for use in reel-fed wrap-around labeling applications where superior graphics are desired.Availability: Africa & M..
Film Tensile Strength at Break, TD 155 MPa
22500 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Label-Lyte™ 38LW280 OPP Film
Product Description: A super white opaque slip controlled, biaxially oriented polypropylene film, metalized on one side. Designed for use in reel-fed wrap-around applications, where outstanding meta..
Film Tensile Strength at Break, TD 155 MPa
22500 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Label-Lyte™ 47LL247 OPP Film
Product Description: A super white opaque, high gloss, cavitated BOPP film designed for use in reel-fed wrap-around labeling applications where superior graphics are desired.Availability: Africa & M..
Film Tensile Strength at Break, TD 155 MPa
22500 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Label-Lyte™ 47LTL247 OPP Film
Product Description: A super white opaque, high gloss, cavitated BOPP film designed for use in reel-fed wrap-around labeling applications where superior graphics are desired. 47LTL247 with supplied ..
Film Tensile Strength at Break, TD 155 MPa
22500 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Metallyte™ 38ICE M OPP Film
Product Description: A coextruded super white opaque, low density, biaxially oriented polypropylene film, metalized on one side. This film is designed for HFFS applications, heat seal or cold seal.A..
Film Tensile Strength at Break, TD 155 MPa
22500 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Metallyte™ 38MW280 OPP Film
Product Description: A super white opaque biaxially oriented polypropylene film, metalized on one side. Ideal for single web packaging applications on HFFS in combination with cold seal.Availability..
Film Tensile Strength at Break, TD 155 MPa
22500 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Metallyte™ 38MW480 OPP Film
Product Description: A super white opaque biaxially oriented polypropylene film, metalized on one side.Availability: Africa & Middle East, Asia Pacific and EuropeKey Features: Outstanding opacity an..
Film Tensile Strength at Break, TD 155 MPa
22500 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Oppalyte™ 30MW648 OPP Film
Product Description: A high speed super white opaque, biaxially oriented polypropylene film coated one side acrylic, one side very low temperature seal (VTLS) coating. VLTS coating provides an excel..
Film Tensile Strength at Break, TD 155 MPa
22500 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Oppalyte™ 35MW647 OPP Film
Product Description: A super white opaque biaxially oriented polypropylene film acrylic coated two sides. Provides outstanding performances on all types of packaging machines.Availability: Africa & ..
Film Tensile Strength at Break, TD 155 MPa
22500 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Oppalyte™ 38ICE OPP Film
Product Description: A coextruded white opaque, low density, biaxially oriented polypropylene film. This film is designed for the ice cream applications, and is suitable for heat seal and cold seal ..
Film Tensile Strength at Break, TD 155 MPa
22500 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Oppalyte™ 38MO447 OPP Film
Product Description: A coextruded white opaque, low density, biaxially oriented polypropylene film, heat sealable on the inside. The treated layer must be printed and varnished to provide the necess..
Film Tensile Strength at Break, TD 155 MPa
22500 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Oppalyte™ 38MW247 OPP Film
Product Description: A super white opaque biaxially oriented polypropylene film. It is designed for use in cold seal applications where superior optics and graphics are desired.Availability: Africa ..
Film Tensile Strength at Break, TD 155 MPa
22500 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Oppalyte™ 40MW648 OPP Film
Product Description: A high speed super white opaque, biaxially oriented polypropylene film coated one side acrylic, one side very low temperature seal (VLTS) coating. VLTS coating provides an excel..
Film Tensile Strength at Break, TD 155 MPa
22500 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Oppalyte™ 45MW647 OPP Film
Product Description: A super white opaque biaxially oriented polypropylene film acrylic coated two sides. Acrylic provides excellent aroma barrier and excellent support for printing. The film provid..
Film Tensile Strength at Break, TD 155 MPa
22500 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Oppalyte™ 47MW247 OPP Film
Product Description: A super white opaque biaxially oriented polypropylene film. It is designed for use in cold seal applications where superior optics and graphics are desired.Availability: Africa ..
Film Tensile Strength at Break, TD 155 MPa
22500 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Oppalyte™ 33ICE OPP Film
Product Description: Coextruded white opaque, low density, biaxially oriented polypropylene film. This film is designed for the ice cream applications, and is suitable for heat seal and cold seal on..
Film Tensile Strength at Break, TD 155 MPa
22500 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Oppalyte™ 33MW247 OPP Film
Product Description: A super white opaque biaxially oriented polypropylene film. It is designed for use in cold seal applications where superior optics and graphics are desired.Availability: Africa ..
Film Tensile Strength at Break, TD 155 MPa
22500 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Oppalyte™ 40MW647 OPP Film
Product Description: A super white opaque, biaxially oriented polypropylene film acrylic coated two sides. Provides outstanding performance on all types of packaging machines.Availability: Africa & ..