Polymer Property : Film Tensile Strength at Break, TD = 16000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 110 MPa

@Thickness 0.250 mm
16000 psi

@Thickness 0.00984 in
ISO 527
Victrex® APTIV® 1000-050 Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline
APTIV PEEK 1000 series films are the unfilled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications.APTI..
Film Tensile Strength at Break, TD 110 MPa
16000 psi
ISO 527
Victrex® APTIV® 1300-050G Polyetheretherketone (PEEK) Polymer Film
DescriptionAPTIV® 1300 film is the black version of unfilled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance ..
Film Tensile Strength at Break, TD 110 MPa
16000 psi
ASTM D882
Dow Saran® 18L-WP White Plastic Barrier Film
Saran™ 18L-WP is a white biaxially oriented monolayer barrier film, preshrunk for lamination applications. It is available in 75 gauge, as single or double wound rolls.Information provided by Dow
Film Tensile Strength at Break, TD 110 MPa
16000 psi
ASTM D882
Dow Saran® 540 Vapor Retarder Film
Saran™ Vapor Retarder Film is a biaxially oriented barrier film designed as a water vapor retarder for insulation applications. It is available in 400 gauge. Roll size: 35.5" x 375 long.Informat..
Film Tensile Strength at Break, TD 110 MPa
16000 psi
ISO 527
Victrex® APTIV® 1300-100G Polyetheretherketone (PEEK) Polymer Film
DescriptionAPTIV® 1300 film is the black version of unfilled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance ..