Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 179 MPa | 26000 psi | ASTM D882 |
DuPont Teijin Films Mylar® M45 Polyester Film, 50 Gauge (15 µm), PVDC Coated
(discontinued **) Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, dispersion coated on one side with a PVDC copolymer. The coating is an excellent moisture and oxygen barrier. M45.. |
|||
Film Tensile Strength at Break, TD | 179 MPa | 26000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 475 Polyester Film, 200 Gauge Melinex® 475 is a high yield, translucent polyester film with superb handling properties. Both surfaces are pretreated to promote adhesion to most industrial coatings.General Product Info: This fil.. |
|||
Film Tensile Strength at Break, TD | 179 MPa | 26000 psi | ASTM D882A |
DuPont Teijin Films Mylar® EC Polyester Film, 300 Gauge Mylar® EC films are electrical grade films designed for use in applications where improved dimensional stability is required. In addition to lower levels of shrinkage, Mylar® EC films offer outsta.. |
|||
Film Tensile Strength at Break, TD | 179 MPa | 26000 psi | ASTM D882A |
DuPont Teijin Films Mylar® EC Polyester Film, 400 Gauge Mylar® EC films are electrical grade films designed for use in applications where improved dimensional stability is required. In addition to lower levels of shrinkage, Mylar® EC films offer outsta.. |
|||
Film Tensile Strength at Break, TD | 179 MPa | 26000 psi | ASTM D882A |
DuPont Teijin Films Mylar® P25 Polyester Film, 50 Gauge Product Description: Mylar® P25 is an uncoated, transparent polyester packaging film designed to be combined with a sealant layer, where the resulting structure will be shallow draw thermoformed. S.. |
|||
Film Tensile Strength at Break, TD | 179 MPa | 26000 psi | ASTM D882A |
DuPont Teijin Films Mylar® P25 Polyester Film, 75 Gauge Product Description: Mylar® P25 is an uncoated, transparent polyester packaging film designed to be combined with a sealant layer, where the resulting structure will be shallow draw thermoformed. S.. |
|||
Film Tensile Strength at Break, TD | 179 MPa | 26000 psi | ASTM D882A |
DuPont Teijin Films Mylar® P25T Polyester Film, 50 Gauge Product Description: Mylar® P25T is a transparent polyester packaging film designed to be combined with a sealant layer, where the resulting structure will be shallow draw thermoformed. It has a co.. |
|||
Film Tensile Strength at Break, TD | 179 MPa | 26000 psi | ASTM D882A |
DuPont Teijin Films Mylar® P25T Polyester Film, 75 Gauge Product Description: Mylar® P25T is a transparent polyester packaging film designed to be combined with a sealant layer, where the resulting structure will be shallow draw thermoformed. It has a co.. |
|||
Film Tensile Strength at Break, TD | 179 MPa | 26000 psi | ASTM D882 |
DuPont Teijin Films Mylar® M45 Polyester Film, 75 Gauge (22 µm), PVDC Coated
(discontinued **) Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, dispersion coated on one side with a PVDC copolymer. The coating is an excellent moisture and oxygen barrier. M45.. |
|||
Film Tensile Strength at Break, TD | 179 MPa | 26000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Oppalyte™ 30 HM-3 OPP Film Product Description: A white opaque OPP film with a proprietary cavitated core. HM-3 is designed for cold seal applications and is used as a surface print, monoweb, or as the inside of lamination. I.. |
|||
Film Tensile Strength at Break, TD | 179 - 248 MPa | 26000 - 36000 psi | Average value: 217 MPa Grade Count:10 |
Overview of materials for Polyvinyl Dichloride (PVDC) Coated Polyester Film This property data is a summary of similar materials in the MatWeb database for the category "Polyvinyl Dichloride (PVDC) Coated Polyester Film". Each property range of values reported is minimum an.. |