Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 15.0 - 18.0 MPa
2180 - 2610 psi
Average value: 17.0 MPa Grade Count:3
Overview of materials for Ethylene Butyl Acrylate
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Butyl Acrylate". Each property range of values reported is minimum and maximum values of approp..