Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 18.6 - 284 MPa
2700 - 41100 psi
Average value: 32.9 MPa Grade Count:80
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Butene, Film
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Butene, Film". Each property range of values reported is minimum..
Film Tensile Strength at Break, TD 18.6 MPa
2700 psi
ASTM-D882
Westlake EB171 MDPE Medium Density Polyethylene
Westlake EF171 is a MDPE resin suggested for use in shrink packaging applications. This material has good TD shrinkage, good optical properties, excellent machinability, and toughness. This resin gr..
Film Tensile Strength at Break, TD 18.6 MPa
2700 psi
ASTM D882
Westlake EF378 Low Density Polyethylene
WESTLAKE EF378 is suggested for cast film applications. It has excellent haze and gloss, good strength, good processability, and good heat sealability.Application/UsesDiaper linersGeneral purpose cl..
Film Tensile Strength at Break, TD 18.6 MPa
2700 psi
ASTM D882
Westlake EF412 Low Density Polyethylene
WESTLAKE polyethylene EF412 is a low-density polyethylene with very good optical and strength properties. This material is an excellent choice for bakery films and food packaging applications.Applic..
Film Tensile Strength at Break, TD 18.6 MPa
2700 psi
ASTM D882
Westlake EF418 Low Density Polyethylene
WESTLAKE polyethylene EF418 is a LDPE formula with excellent optical properties suggested by light and medium duty packaging.Application/UsesLight and medium duty produce bagsClarity packagingGenera..
Film Tensile Strength at Break, TD 18.6 MPa
2700 psi
ASTM D882
Westlake EF421 Low Density Polyethylene
WESTLAKE polyethylene EF421 is a low-density polyethylene with very good optical and strength properties. This material is an excellent choice for bakery films and general purpose food packaging app..
Film Tensile Strength at Break, TD 18.6 MPa
2700 psi
ASTM D882
Westlake EF601 Low Density Polyethylene
Westlake EF601 is a fractional melt LDPE with excellent toughness. It is suggested in heavy duty films and shipping sacks, and in industrial shrink applications. It can be used as a bubble stabilize..
Film Tensile Strength at Break, TD 18.6 MPa
2700 psi
ASTM D882
Westlake EF796 Low Density Polyethylene
Westlake Polyethylene EF796 is a low density formulation suggested for film applications requiring a good balance of properties such as converter film for industrial packaging and general-purpose pa..
Film Tensile Strength at Break, TD 18.6 MPa
2700 psi
ASTM D882
Westlake EF923 Low Density Polyethylene
Westlake Polyethylene EF923 is a low density formulation suggested for film applications that require a good balance of properties such as converter film for industrial packaging and general purpose..
Film Tensile Strength at Break, TD 18.6 MPa
2700 psi
ASTM D882
Westlake EN923 Low Density Polyethylene
Westlake Polyethylene EN923 is a low density formulation suggested for film applications where enhanced processability and high clarity are required. It is characterized by good tear strength, impa..
Film Tensile Strength at Break, TD 18.6 MPa
2700 psi
ASTM D882
Formosa Plastics Formolene® L42022B Film (Butene Grade) LLDPE
Butene Copolymer (Barefoot)Applications: Blown and cast filmBlown and cast filmMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of p..
Film Tensile Strength at Break, TD 18.6 MPa
2700 psi
ASTM D882
Formosa Plastics Formolene® L42022E2 Film (Butene Grade) LLDPE
Butene Copolymer (Low slip and antiblock)Applications: Thin gauge blown filmThin gauge blown filmMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, cove..
Film Tensile Strength at Break, TD 18.6 MPa
2700 psi
ASTM D882
ExxonMobil LD 124.MS General Purpose Clarity Film Resin
Product Description: LD 124.MS blown film resin offers an excellent balance of optical and strength properties for general purpose clear film applications. Availability: Latin America, North America..
Film Tensile Strength at Break, TD 18.6 MPa
2700 psi
ASTM D882
ExxonMobil LD 129.24 Cast Overwrap Film Resin
Product Description: LD 129.24 is a medium density homopolymer film resin with good clarity and excellent stiffness. Film made from LD 129.24 can be used in overwrap applications and in push-through..
Film Tensile Strength at Break, TD 18.6 MPa
2700 psi
ASTM D882
ExxonMobil LDPE LD 124.MS Low Density Polyethylene Resin
Product Description: LD 124.MS blown film resin offers an excellent balance of optical and strength properties for general purpose clear film applications. Availability: Latin America, North America..
Film Tensile Strength at Break, TD 18.6 MPa
2700 psi
Dow LDPE 768A Low Density Polyethylene, Film Grade
DOW LDPE 768A resin is a medium density film resin with additional stabilization for films requiring high modulus such as paper overwrap. It contains low levels of both slip additive and antiblock a..
Film Tensile Strength at Break, TD 18.6 MPa

@Thickness 0.0356 mm
2700 psi

@Thickness 0.00140 in
ASTM D-882
Bapolene® 270F Low Density Polyethylene Film Extrusion Resin
Bapolene® 270F is an LDPE for blown film requiring superior clarity. It contains 1600 ppm antiblock and 725 ppm slip additives. This product meets the Food and Drug Administration requirements of ..