Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 180.33 MPa
26154 psi
510
ExxonMobil Digilyte® 65 EW-214 Coated, White Opaque OPP Facestock
White, polypropylene, pressure-sensitive, label facestock designed to be printed on an Indigo® Omnius® One-Shot Color™ press. This film offers strength and opacity. The ElectroInk® receptive c..