Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 180.33 MPa | 26154 psi | 510 |
ExxonMobil Digilyte® 65 EW-214 Coated, White Opaque OPP Facestock White, polypropylene, pressure-sensitive, label facestock designed to be printed on an Indigo® Omnius® One-Shot Color™ press. This film offers strength and opacity. The ElectroInk® receptive c.. |