Polymer Property : Film Tensile Strength at Break, TD = 1890 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 13.0 MPa
1890 psi
ASTM D882
Huntsman PE5050 Extrusion Coating Polyethylene  (discontinued **)
Homopolymer, Drug Master File listed product, and FDA compliant.Features: High draw down, low neck-in, excellent heat sealability, and excellent adhesion.Applications: Extrusion: coating grade and t..
Film Tensile Strength at Break, TD 13.0 - 39.0 MPa
1890 - 5660 psi
Average value: 23.9 MPa Grade Count:9
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade". Each property range of values reported..
Film Tensile Strength at Break, TD 13.0 - 40.0 MPa
1890 - 5800 psi
Average value: 24.4 MPa Grade Count:138
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum a..
Film Tensile Strength at Break, TD 13.0 MPa
1890 psi
ASTM D882
SCG Chemicals EL-Leneâ„¢ L2020F Linear Low Density Polyethylene Film
Key Characteristics:High output and elongationContains 1800 ppm slip agent and 1400 ppm antiblocking agentRecommended Applications:General purpose bag, cast film, small bag, merchandise bag, printed..