Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 13.0 - 39.0 MPa
1890 - 5660 psi
Average value: 23.9 MPa Grade Count:9
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade". Each property range of values reported..
Film Tensile Strength at Break, TD 33.0 - 39.0 MPa
4790 - 5660 psi
Average value: 36.7 MPa Grade Count:3
Overview of materials for High Density Polyethylene (HDPE), Copolymer Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Copolymer Film Grade". Each property range of values reported is minim..