Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 331 Polyester Film, 200 Gauge Melinex® 331 is an opaque, pearlescent, white film with excellent handling properties that is pretreated on one side to promote adhesion to most industrial coatings.Approvals: UL Recognition - Prod.. |
|||
Film Tensile Strength at Break, TD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 331 Polyester Film, 300 Gauge Melinex® 331 is an opaque, pearlescent, white film with excellent handling properties that is pretreated on one side to promote adhesion to most industrial coatings.Approvals: UL Recognition - Prod.. |
|||
Film Tensile Strength at Break, TD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 331 Polyester Film, 700 Gauge Melinex® 331 is an opaque, pearlescent, white film with excellent handling properties that is pretreated on one side to promote adhesion to most industrial coatings.Approvals: UL Recognition - Prod.. |
|||
Film Tensile Strength at Break, TD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 331W Polyester Film, 200 Gauge An opaque, pearlescent, white film with excellent handling properties that is pretreated on one side to promote adhesion to most industrial coatings. 331W has same properties as 331 with the only ex.. |
|||
Film Tensile Strength at Break, TD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 513P Polyester Film, 650 Gauge Melinex® 513P is a high clarity, knurled film with excellent handling properties that is pretreated on both sides to promote adhesion to most industrial coatings.General Product Info: Melinex® 513.. |
|||
Film Tensile Strength at Break, TD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 618 Polyester Film, 1000 Gauge Melinex® 618 is a super clear polyester film, pretreated on one side to promote adhesion. It is a high clarity, non-yellow base with excellent adhesion on the pretreated surface. Used for a wide ra.. |
|||
Film Tensile Strength at Break, TD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 623 Polyester Film, 1000 Gauge Melinex® 623 is a super clear polyester film pretreated on both surfaces to give superior solvent adhesion and improved handleability.Information provided by DuPont. |
|||
Film Tensile Strength at Break, TD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 725 Polyester Film Melinex® 725 is a high clarity polyester film pretreated on both sides to promote adhesion to many industrial coatings and inks. Melinex® 725 exhibits improved performance in multi-pass printing a.. |
|||
Film Tensile Strength at Break, TD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Mylar® 851H Polyester Film, 60 Gauge Mylar® 851H (also called Mylar® 851) is a co-extruded, one side amorphous, heat sealable polyester film designed to be used in metallization, print, and lamination applications. This film is suita.. |
|||
Film Tensile Strength at Break, TD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Mylar® E Polyester Film, 142 Gauge Mylar® E polyester film is a clear smooth base film engineered to provide superior optical and physical properties required of critical dying, metallizing, laminating, labeling and coating applicat.. |
|||
Film Tensile Strength at Break, TD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Mylar® E Polyester Film, 200 Gauge Mylar® E polyester film is a clear smooth base film engineered to provide superior optical and physical properties required of critical dying, metallizing, laminating, labeling and coating applicat.. |
|||
Film Tensile Strength at Break, TD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Mylar® E Polyester Film, 300 Gauge Mylar® E polyester film is a clear smooth base film engineered to provide superior optical and physical properties required of critical dying, metallizing, laminating, labeling and coating applicat.. |
|||
Film Tensile Strength at Break, TD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Mylar® E Polyester Film, 92 Gauge Mylar® E polyester film is a clear smooth base film engineered to provide superior optical and physical properties required of critical dying, metallizing, laminating, labeling and coating applicat.. |
|||
Film Tensile Strength at Break, TD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Mylar® OWF2 Polyester Film, 60 Gauge Product Description: Mylar® OWF2 is a co-extruded, one side amorphous, heat sealable polyester film designed to be used as an overwrap film. Mylar® OWF2 has a thicker heat sealable layer than Myla.. |
|||
Film Tensile Strength at Break, TD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 680 Polyester Film, 1000 Gauge Melinex® 680 is a super clear polyester film, pretreated on one side to promote adhesion with improved handleability. It is high clarity, non-yellow base with excellent adhesion on the pretreated s.. |