Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 23.1 MPa
3350 psi
ASTM D882
NOVA Chemicals Novapol® LF-Y320-C Fractional Melt LDPE Film Resin
Features: High melt strength and superior bubble stabilityEnhances throughputs in LLDPE blendsSuperior strength and toughnessExcellent shrink film characteristics Applications: Industrial packagingL..
Film Tensile Strength at Break, TD 23.1 MPa
3350 psi
ASTM D882
NOVA Chemicals Novapol® LF-Y320-D Fractional Melt LDPE Film Resin
Features: High melt strength and superior bubble stabilityEnhances throughputs in LLDPE blendsSuperior strength and toughnessExcellent shrink film characteristics Applications: Industrial packagingL..
Film Tensile Strength at Break, TD 23.1 MPa
3350 psi
ASTM D882
ExxonMobil Pax-Plus™ 3201 Blown Film Resin
Pax-Plus 3201 is a rubber modified high density polyethylene film resin that exhibits excellent impact strength and stress crack resistance. It is used primarily in film where its good tear resista..