Polymer Property : Film Tensile Strength at Break, TD = 38.2 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 38.2 MPa
5540 psi
Kuraray HYBRAR® CF2 Mono Layer Cast Film
Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb..
Film Tensile Strength at Break, TD 38.2 MPa
5540 psi
ASTM D882
ExxonMobil LL 3001.32 Cast Film Resin
Product Description: LL 3001.32 is a hexane copolymer LLDPE designed for the blown or cast film process. Films made from LL 3001.32 have outstanding tensile and toughness properties. The superior st..