ExxonMobil LL 3001.32 Cast Film Resin

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer Exxon Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil LL 3001.32 Cast Film Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: LL 3001.32 is a hexane copolymer LLDPE designed for the blown or cast film process. Films made from LL 3001.32 have outstanding tensile and toughness properties. The superior strength properties, along with excellent drawability, make this a very versatile packaging film resin.Availability: Latin America, North America and South America Additive: Antiblock: NoSlip: NoProcessing Aid: No Thermal Stabilizer: YesApplications: Freezer FilmHeavy Duty BagsIce BagsTrash Bags Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.917 g/cc
0.0331 lb/in³
ExxonMobil Method
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 8.41 MPa
1220 psi
ASTM D882
Film Tensile Strength at Yield, TD 7.72 MPa
1120 psi
ASTM D882
Film Elongation at Break, MD 340 %
340 %
ASTM D882
Film Elongation at Break, TD 790 %
790 %
ASTM D882
Puncture Energy 3.28 J
2.42 ft-lb
ExxonMobil
Elmendorf Tear Strength, MD 11.8 g/micron
300 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 29.53 g/micron
750.0 g/mil
ASTM D1922
Dart Drop 3.15 g/micron
80.0 g/mil
ASTM D1709
Film Tensile Strength at Break, MD 66.1 MPa
9590 psi
ASTM D882
Film Tensile Strength at Break, TD 38.2 MPa
5540 psi
ASTM D882
1% Secant Modulus, MD 119 MPa
17300 psi
ASTM D882
1% Secant Modulus, TD 145 MPa
21000 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point 124 °C
255 °F
Peak Melting Temperature; ExxonMobil Method
Optical Properties Metric English Comments
Haze 2.2 %
2.2 %
ASTM D1003
Gloss 89 %
89 %
45°; ASTM D2457
Descriptive Properties Value Comments
Features Thermal Stabilizer