Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 57.9 MPa | 8400 psi | ASTM D822 |
LG Chemical LUTENE-H FE0070 HDPE LUTENE-H FE0070 is mainly intended for the extrusion of blown film with high mechanical properties for the manufacture of "T-Shirt" grocery sacks, can liners. Especially, LUTENE-H FE0070 resin can b.. |
|||
Film Tensile Strength at Break, TD | 57.9 MPa | 8400 psi | ASTM D882 |
ExxonMobil Exceed™ 1518HA Metallocene Polyethylene Resin Product Description: Exceed 1518HA is a metallocene ethylene-hexene copolymer. Films made from Exceed 1518HA have outstanding tensile, impact strength and puncture. These superior strength propertie.. |