Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Exceed™ 1518HA Metallocene Polyethylene Resin

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Exxon Chemical
Trade Name Exceed™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Exceed™ 1518HA Metallocene Polyethylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Exceed 1518HA is a metallocene ethylene-hexene copolymer. Films made from Exceed 1518HA have outstanding tensile, impact strength and puncture. These superior strength properties, along with excellent drawability, makes this a very versatile packaging film. Availability: Latin America, North America and South AmericaAdditive:Antiblock: NoSlip: NoProcessing Aid: YesThermal Stabilizer: YesApplications: Bag in BoxBarrier Food PackagingBlown FilmBlown Stretch FilmFood packaging Form Fill and Seal Packaging General PackagingHeavy Duty Bags Ice Bags Packaging FilmsPremium Trash Bags Stand Up Pouches Information provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.918 g/cc
0.0332 lb/in³
ExxonMobil method
Melt Flow 1.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 8.96 MPa
1300 psi
ASTM D882
Film Tensile Strength at Yield, TD 9.65 MPa
1400 psi
ASTM D882
Film Elongation at Break, MD 550 %
550 %
ASTM D882
Film Elongation at Break, TD 690 %
690 %
ASTM D882
Puncture Energy 4.07 J
3.00 ft-lb
ExxonMobil Method
Elmendorf Tear Strength MD 290 g
290 g
ASTM D1922
Elmendorf Tear Strength TD 420 g
420 g
ASTM D1922
Dart Drop Test 640 g
1.41 lb
ASTM D1709
Film Tensile Strength at Break, MD 63.4 MPa
9200 psi
ASTM D882
Film Tensile Strength at Break, TD 57.9 MPa
8400 psi
ASTM D882
1% Secant Modulus, MD 179 MPa
26000 psi
ASTM D882
1% Secant Modulus, TD 193 MPa
28000 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point <= 244 °C
<= 471 °F
Peak Melting Point; ExxonMobil method
Optical Properties Metric English Comments
Haze 40 %
40 %
ASTM D1003
Gloss 20 %
20 %
45°; ASTM D2457
Descriptive Properties Value Comments
Puncture Force 11 lbf
ExxonMobil Method