Polymer Property : Film Tensile Strength at Break, TD = 6820 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 47.0 MPa
6820 psi
ASTM D 882
NOVA Chemicals Sclair® FPr017-D Octene LLDPE Film Resin
FPr017-D complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. FPr0..
Film Tensile Strength at Break, TD 47.0 MPa
6820 psi
ASTM D882-02
Ipiranga Petrochem LB 0120 BS LLDP
IPQ produces Linear Low Density Polyethylene (LLDPE) for use by plastics molding industry segments that employ extrusion processes in the manufacturing of films destined for producing bobbins and ba..
Film Tensile Strength at Break, TD 47.0 MPa
6820 psi
ASTM D882-02
Ipiranga Petrochem LTH 0212 LLDP
IPQ produces Linear Low Density Polyethylene (LLDPE) for use by plastics molding industry segments that employ extrusion processes in the manufacturing of films destined for producing bobbins and ba..
Film Tensile Strength at Break, TD 47.0 MPa
6820 psi
ASTM D882
M. Holland Company MAGMA® LM311-DX LLDPE  (discontinued **)
Features: Good Processability, Good Puncture Resistance, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland.
Film Tensile Strength at Break, TD 47.0 MPa
6820 psi
ASTM D882
NOVA Chemicals Sclair® 11C1 Octene LLDPE Film Resin  (discontinued **)
Low gel, Good processability, Excellent mechanical propertiesApplications: Shrink filmAdditives: Process stabilizerFilm properties are typical of blown film extruded at a blowup ratio of 2.5:1, but ..