Polymer Property : Flexural Yield Strength = 20300 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 7.00 - 140 MPa
1020 - 20300 psi
Average value: 74.9 MPa Grade Count:39
Overview of materials for Nylon 66/6
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb ..
Flexural Yield Strength 11.0 - 140 MPa
1600 - 20300 psi
Average value: 93.6 MPa Grade Count:197
Overview of materials for Nylon 66, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Flexural Yield Strength 29.9922 - 140 MPa

@Temperature -40.0 - 90.0 °C
4350.01 - 20300 psi

@Temperature -40.0 - 194 °F
Average value: 71.0 MPa Grade Count:4
Overview of materials for Nylon 66, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Flexural Yield Strength 38.0 - 140 MPa

@Temperature -40.0 - 80.0 °C
5510 - 20300 psi

@Temperature -40.0 - 176 °F
Average value: 86.8 MPa Grade Count:2
Overview of materials for Nylon 66, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum ..
Flexural Yield Strength 70.0 - 140 MPa
10200 - 20300 psi
Average value: 101 MPa Grade Count:22
Overview of materials for Melamine-Phenolic Copolymer
This property data is a summary of similar materials in the MatWeb database for the category "Melamine-Phenolic Copolymer". Each property range of values reported is minimum and maximum values of ap..
Flexural Yield Strength 134 - 140 MPa

@Temperature 80.0 - 80.0 °C
19400 - 20300 psi

@Temperature 176 - 176 °F
Average value: 137 MPa Grade Count:4
Overview of materials for Polypropylene with 60% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 60% Glass Fiber Filler". Specific grades with glass content between 55% and 64% are i..