Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 83.6 MPa | 12100 psi | ASTM D790 |
RedEye On Demand VeroBlue PolyJet™ FC840 for Rapid Prototyping Vero PolyJet Resin (VeroBlue™ FC840 & VeroBlack™ FC870) is a photopolymer resin designed for precise jetting in super fine layers by PolyJet™ Technology, often used in rapid prototyping. Our Vero.. |
|||
Flexural Yield Strength | 83.4 MPa @Thickness 3.20 mm |
12100 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical LG704W ABS, Low Gloss, Heat Resistance Feature: Injection Molding, Low Gloss, Heat ResistanceApplication: Automobiles Interior Housing (Column Cover, Filllar Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by LG Chem.. |
|||
Flexural Yield Strength | 83.4 MPa @Thickness 3.20 mm |
12100 psi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUMAX GP5106FI PBT+ABS+GF10%, Flame Retardant Description: Injection Molding Grade, PBT+ABS+GF10%, Flame Retardant, Impact Modified, Dimensional StabilityApplication: E&E (Switch)CAS: 9003-56-9, 68928-70-1, 65997-17-3, 24968-12-5, 9003-54-7 an.. |
|||
Flexural Yield Strength | 83.4 MPa @Thickness 3.20 mm |
12100 psi @Thickness 0.126 in |
2.8mm/min; ASTM D790 |
LG Chemical LUMID HI1102A(W) PA6, High Impact Feature: Injection Molding, PA6, High ImpactApplication: H/Lamp Screw MountingCAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical |
|||
Flexural Yield Strength | 83.4 MPa @Thickness 6.40 mm |
12100 psi @Thickness 0.252 in |
1.3mm/min; ASTM D790 |
LG Chemical LUPOL GP2150 PP+GF15% Description: Injection Molding, PP+GF15%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 65997-17-3Information provided by LG Chemical |
|||
Flexural Yield Strength | 83.4 MPa @Thickness 6.40 mm |
12100 psi @Thickness 0.252 in |
1.3mm/min; ASTM D790 |
LG Chemical LUPOL HI2202B PP+GF20%, High Impact Description: Injection Molding, PP+GF20%, General Purpose, High ImpactApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0, 65997-17-3 and 9010-79-1Information provided by LG Chemica.. |
|||
Flexural Yield Strength | 83.4 MPa | 12100 psi | ASTM D570 |
LG Chemical Lupox® PBT-GP-1000 High Flow PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 83.4 MPa @Thickness 3.20 mm |
12100 psi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical Lupox® SG3250M PBT+PET+MF25% Description: Injection Molding, PBT+PET+MF25%, Good SurfaceApplication: Automotive (Head Lamp Bezel)CAS No. 24968-12-5, 25038-59-9 and 14807-96-6Information provided by LG Chemical |
|||
Flexural Yield Strength | 83.4 MPa @Thickness 3.20 mm |
12100 psi @Thickness 0.126 in |
2.8mm/min; ASTM D790 |
LG Chemical Lupox® SV1120M PBT Description: Injection Molding, PBT, General Purpose, High ViscosityApplication: Films & Sheets, Optical Loose TubeCAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Flexural Yield Strength | 83.4 MPa @Thickness 6.40 mm |
12100 psi @Thickness 0.252 in |
50mm/min; ASTM D790 |
LG Chemical Lupox® TE5000H PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional StabilityApplication: Automotive ItemCAS No. 9003-01-04, 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Flexural Yield Strength | 83.4 MPa @Thickness 6.40 mm |
12100 psi @Thickness 0.252 in |
2.5mm/min; ASTM D790 |
LG Chemical Lupox® TE5000HZ PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional StabilityApplication: Automotive (Door Handle)CAS No. 9003-01-04, 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Flexural Yield Strength | 83.4 MPa @Thickness 6.40 mm |
12100 psi @Thickness 0.252 in |
2.5mm/min; ASTM D790 |
LG Chemical Lupox® TE5000LZ PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional Stability, Good WeatherabilityApplication: Automotive (Door Garnish)CAS No. 9003-01-04, 24968-12-5 and 103598-77-2Information provide.. |
|||
Flexural Yield Strength | 83.4 MPa | 12100 psi | ASTM D790 |
Techmer ES Luriblend® PC MRX BK Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 83.4 MPa | 12100 psi | ASTM D790 |
Techmer ES Luriblend® TPX-PPO/HIPS-02072 BK Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: Lubricated, Good Wear Resistance, Low Friction and HomopolymerUL File Number: E157318Information provided by TP Composites,.. |
|||
Flexural Yield Strength | 83.4 MPa | 12100 psi | ASTM D790 |
Samyang Tribit® 1500 Polybutylene Terephthalate Characteristics:Medium viscosityApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll information provided by Samy.. |
|||
Flexural Yield Strength | 83.4 MPa | 12100 psi | ASTM D790 |
Samyang Triloy® 210NHF Polymer Alloy, Flame Retardancy (Non-Halogen) Excellent impact, formability and weather resistance.210NHF is a flame retardant (non-halogen) grade.Applications: LCD TV Rear Cover (high flow)Information provided by Samyang. |
|||
Flexural Yield Strength | 83.4 MPa | 12100 psi | ASTM D790 |
Samyang Triloy® 215 PC/ABS alloy Characteristics:Dimensional stabilityHigh heat resistanceGood flowApplications:Camera partsExterior panelCluster fasciaWheel coverStructural applicationI/P. core panelHelmet shellGlove box doorCowl .. |
|||
Flexural Yield Strength | 83.4 MPa | 12100 psi | ASTM D790 |
Samyang Trimma® FT6125 I[R] PMMA, Transparent High transparency and high scratch resistance. Stable against weak acids, strong acids, weak alkalis and inorganic salts.Information provided by Samyang. |
|||
Flexural Yield Strength | 83.4 MPa | 12100 psi | ASTM D790 |
Samyang Trirex® DMF3000S Polycarbonate, Anti-yellowing PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.DMF3000S is an anti-yellowing grade.Information provided by Samyang. |
|||
Flexural Yield Strength | 83.4 MPa | 12100 psi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® D201 PBT Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Yield Strength | 83.4 MPa | 12100 psi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® T101 PET Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Yield Strength | 83.4 MPa | 12100 psi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® N602 Nylon 66 Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Yield Strength | 83.4 MPa | 12100 psi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® N602 Nylon 66 Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Yield Strength | 83.4 MPa @Thickness 6.40 mm |
12100 psi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron IMC-45M ABS-PC Alloy ABS-polycarbonate alloys for High service temperature applications.Information provided by Bhansali |
|||
Flexural Yield Strength | 83.4 MPa | 12100 psi | ASTM D790 |
Cheng Yu Plastic 3255 TPE Rubber |
|||
Flexural Yield Strength | 83.4 MPa @Thickness 6.40 mm |
12100 psi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron IMC-45M ABS-PC Alloy ABS-polycarbonate alloys for High service temperature applications.Information provided by Bhansali |
|||
Flexural Yield Strength | 83.2 MPa | 12100 psi | ASTM D790 |
Plenco 6554 Phenolic, Granular, Compression Molded
(discontinued **) Two-Stage Phenolic. PLENCO 06554 is an organic reinforced phenolic molding compound modified with PTFE to offer improved coefficient of friction values. 06554 is available in black.Information supp.. |
|||
Flexural Yield Strength | 83.4 MPa | 12100 psi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® D201 PBT Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Yield Strength | 83.4 MPa | 12100 psi | DIN 53455; ASTM D790 |
Kolon SPELLOY® KB133HF PC + PBT Alloy Resin
(discontinued **) SPELLOY® is a new technology of thermoplastic Polymer alloys developed to provide unique combination of excellent mechanical properties.High impact resistance (at low temperature), good dimensional.. |
|||
Flexural Yield Strength | 83.5 MPa | 12100 psi | 15 mm/min; ASTM D790 |
LG Chemical 15NFI GPPS High flow, Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Heat resistance and chemical resistance, Superio.. |