Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 91.0 MPa | 13200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 943 PC Opaque colors, medium viscosity, superior flame retardance. UV-stabilized. |
|||
Flexural Yield Strength | 91.0 MPa | 13200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 943ASR PC More robust design of standard 900 series flame retardant grade. Internal mold release. UV-stabilized. |
|||
Flexural Yield Strength | 91.0 MPa | 13200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 950 PC Opaque colors, high viscosity, superior flame retardance. |
|||
Flexural Yield Strength | 91.0 MPa | 13200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL4016 PC Copolymer (Asia Pacific) 6% GF reinforced opaque polycarbonate-siloxane copolymer, for increased stiffness with good impact strength. Improved release properties. Available in limited colors only.This data was supplied by S.. |
|||
Flexural Yield Strength | 91.0 MPa | 13200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL8414 PC Copolymer Lexan* EXL8414 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and up to 25% post consumer recycle content. Availability of resin is restricted and lead times are.. |
|||
Flexural Yield Strength | 91.0 MPa | 13200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXD9810 PC Copolymer Non-chlorinated, non-brominated Flame retardant PC-siloxane copolymer blend. Excellent processability, super high flow, good impact, UL rated V-0. Limited translucent colors. |
|||
Flexural Yield Strength | 91.0 MPa | 13200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXD9810 PC Copolymer (Asia Pacific) Non-chlorinated, non-brominated Flame retardant PC-siloxane copolymer blend. Excellent processability, super high flow, good impact, UL rated V-0. Limited translucent colors. |
|||
Flexural Yield Strength | 91.0 MPa | 13200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® ML4506 PC Transparent polycarbonate for aircraft applications requiring FAR 25.853a compliance. Injection moldable. |
|||
Flexural Yield Strength | 91.0 MPa | 13200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DL001 PC (Europe-Africa-Middle East) LNP* LUBRICOMP* DL001 is a compound based on Polycarbonate resin containing PTFE. Added features include: Internally Lubricated. |
|||
Flexural Yield Strength | 91.0 MPa | 13200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 920A PC (Asia Pacific) Low viscosity injection moldable, flame retardant PC. Exceptional surface appearance. Clear, tints and opaque colors. |
|||
Flexural Yield Strength | 91.0 MPa | 13200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 920ASR PC More robust design of standard 900 series flame retardant grade. Internal mold release. |
|||
Flexural Yield Strength | 91.0 MPa | 13200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 953 PC Opaque colors, high viscosity, superior flame retardance. UV-stabilized. |
|||
Flexural Yield Strength | 91.0 MPa | 13200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 953 PC (Asia Pacific) Opaque colors, high viscosity, superior flame retardance. UV-stabilized. |
|||
Flexural Yield Strength | 91.0 MPa | 13200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 9925A PC (Asia Pacific) Lexan 9925A is a flame retardant transparent polycarbonate featuring non brominated and non chlorinated FR system with good flow and thin wall FR performance. It intended to meet WEEE/RoHS requireme.. |
|||
Flexural Yield Strength | 91.0 MPa | 13200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL8414 PC Copolymer (Asia Pacific) Lexan* EXL8414 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and 25% post consumer recycle content. Limited availability and restricted color only. Higher color.. |
|||
Flexural Yield Strength | 91.0 MPa | 13200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXD9810 PC Copolymer (Europe-Africa-Middle East) Non-chlorinated, non-brominated Flame retardant PC-siloxane copolymer blend. Excellent processability, super high flow, good impact, UL rated V-0. Limited translucent colors.This data was supplied b.. |
|||
Flexural Yield Strength | 91.0 MPa | 13200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXD9810U PC Copolymer (Asia Pacific) Polycarbonate with high flow, excellent processability, good impact and thermal properties, UV stabilized, non-Chlorine and non-Bromine flame retardant, UL rated V-0 and V-1. Available in limited di.. |
|||
Flexural Yield Strength | 91.0 MPa | 13200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® FXE9925A PC (Asia Pacific) Illuminate / edge glow color effect grade of Lexan 9925A. 9925A is a flame retardant transparent polycarbonate featuring non brominated and non chlorinated FR system with good flow and thin wall FR .. |
|||
Flexural Yield Strength | 91.0 MPa | 13200 psi | ASTM D790 |
Asahi Kasei Tenac®-C 8554 Acetal Copolymer, High Flow
(discontinued **) Superhigh-flow grade, with properties necessary for VCR reels.Applications: VCR reels.This product is not a part of the standard product line dated 2003. |
|||
Flexural Yield Strength | 91.0 MPa | 13200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® ML4539 PC Polycarbonate for aircraft applications requiring FAR 25.853a compliance. Injection moldable. Opaque colors. |
|||
Flexural Yield Strength | 91.2 MPa | 13200 psi | 23°C; 50% RH; ASTM D570 |
LG Chemical Lucet® N127 Acetal Copolymer Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 91.2 MPa @Thickness 3.20 mm |
13200 psi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GN1006FMR PC, Halogen Free, Flame Retardant, Transparency Description: Injection Molding, PC, Halogen Free Flame Retardant, Transparency, Mold ReleaseApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG.. |
|||
Flexural Yield Strength | 91.2 MPa @Thickness 3.20 mm |
13200 psi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GN1006FT PC, Halogen Free, Flame Retardant Description: Injection Molding, PC, Halogen Free Flame Retardant, Good FlowApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
Flexural Yield Strength | 91.0 MPa | 13200 psi | ASTM D790 |
Spartech Royalite R922 PC/ABS Aircraft Grade Sheet Description: Aircraft Grade SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 91.0 MPa | 13200 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl PX0346 PPE+PS This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 91.0 MPa | 13200 psi | ASTM D790 |
Westlake Plastics Radel® R 5500 Polyphenylsulfone Stock shapes extruded from Radel R resins offer a superior combination of high performance properties that include excellent thermal stability, outstanding toughness, and good environmental stress c.. |
|||
Flexural Yield Strength | 91.0 MPa | 13200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 940A PC (Asia Pacific) Medium viscosity, flame retardant PC. Exceptional surface. Clear, tints and opaque colors. |
|||
Flexural Yield Strength | 91.0 MPa | 13200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 950A PC Transparent, clear and colors, high viscosity, flame retardant with exceptional surface. |
|||
Flexural Yield Strength | 91.0 MPa | 13200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 953A PC Clear, tints and opaque colors, high viscosity, flame retardant with exceptional surface. UV-stabilized. |
|||
Flexural Yield Strength | 91.0 MPa | 13200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer (Asia Pacific) 40 MFR LEXAN High Flow Ductile Copolymer |