Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycolac® INP572 ABS High molecular weight SAN, functions as a carrier resin for color concentrates. Can be used as compounding additives for polymer blends. Can be blended with high rubber graft modifier resins to pro.. |
|||
Flexural Yield Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycolac® INP572 ABS+SAN High molecular weight SAN, functions as a carrier resin for color concentrates. Can be used as compounding additives for polymer blends. Can be blended with high rubber graft modifier resins to pro.. |
|||
Flexural Yield Strength | 92.0 MPa | 13300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® CY6009 PC+ABS (Asia Pacific) CY6009 is a flame retardant (FR) PC+ABS blend with non-brominated and non-chlorinated FR systems. Its excellent flow together with balanced properties and thin wall 5VB capability at less than 2 mm.. |
|||
Flexural Yield Strength | 92.0 MPa | 13300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL1414 PC Copolymer (Asia Pacific) Lexan* EXL1414 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductility in combination with excel.. |
|||
Flexural Yield Strength | 92.0 MPa | 13300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL1444 PC Copolymer (Asia Pacific) Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-.. |
|||
Flexural Yield Strength | 92.0 MPa | 13300 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® EXL1464T PC Copolymer Lexan* EXL1464T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo.. |
|||
Flexural Yield Strength | 92.0 MPa | 13300 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® EXL1464T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1464T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo.. |
|||
Flexural Yield Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1880T PC Copolymer (Asia Pacific) Lexan* EXL1880T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, transparent injection molding grade. This resin offers good low temperature (0 C) ductility in combination with very h.. |
|||
Flexural Yield Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1890T PC Copolymer (Asia Pacific) Lexan* EXL1890T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade for food contact applications. This resin offers cold temperature (0 °C) ductility in combin.. |
|||
Flexural Yield Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1890T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1890T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade for food contact applications. This resin offers cold temperature (0 °C) ductility in combin.. |
|||
Flexural Yield Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXD1433T PC Copolymer (Asia Pacific) Clear PC-siloxane copolymer with excellent processability in special light diffusion colors. Medium flow, UV stabilized. Improved toughness compared to standard PC in same color. Color package may .. |
|||
Flexural Yield Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXD1433T PC Copolymer (Europe-Africa-Middle East) Clear PC-siloxane copolymer with excellent processability in special light diffusion colors. Medium flow, UV stabilized. Improved toughness compared to standard PC in same color. Color package may .. |
|||
Flexural Yield Strength | 92.0 MPa | 13300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® FXE1414 PC Copolymer Lexan* FXE1414 polycarbonate (PC) siloxane copolymer resin is a special effects fluorescent, medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductil.. |
|||
Flexural Yield Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPM1914 PC Copolymer (Asia Pacific) High flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). E.. |
|||
Flexural Yield Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPM1914 PC Copolymer (Europe-Africa-Middle East) High flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). E.. |
|||
Flexural Yield Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
Flexural Yield Strength | 92.0 MPa | 13300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® ML7689 PC Copolymer (Asia Pacific) Lexan* ML7689 polycarbonate (PC) siloxane copolymer resin IS a high viscosity injection molding (IM) grade WITH good processability, offering opportunities FOR shorter IM CYCLE times compared TO sta.. |
|||
Flexural Yield Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Faradex NSL121 PC+ABS (Europe-Africa-Middle East) LNP* Faradex* NSL121 is a compound based on PC+ABS Blend resin containing Stainless Steel Fiber, PTFE, Flame Retardant. Added features include: Electrically Conductive, EMI/RFI Shielding, Internall.. |
|||
Flexural Yield Strength | 92.0 MPa | 13300 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycoloy® C6840 PC+ABS (Europe-Africa-Middle East) Cycoloy* C6840 resin is an injection moldable, flame retardant PC/ABS blend. It contains non-chlorinated & non-brominated flame retardant systems intended to meet governmental regulations and variou.. |
|||
Flexural Yield Strength | 92.0 MPa | 13300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL1414T PC Copolymer (Asia Pacific) Lexan* EXL1414T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo.. |
|||
Flexural Yield Strength | 92.0 MPa | 13300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL9414T PC Copolymer (Asia Pacific) Lexan* EXL9414T resin grade is a halogen-free flame retardant polycarbonate featuring transparency, -40 degree C ductility and UL-94 V0 rating for injection molding applications. Excellent impact co.. |
|||
Flexural Yield Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® EH7025AG PBT+PET Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application. |
|||
Flexural Yield Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® EH7025AG PBT+PET (Europe-Africa-Middle East) Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application. |
|||
Flexural Yield Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics XYLEX X7507 PC+POLYESTER (Asia Pacific) F-1 weathering certified in natural color, specially designed for Pool & Spa applications. Currently available in natural color only. |
|||
Flexural Yield Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP (Asia Pacific) Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Yield Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DX02437 PC (Asia Pacific) LNP Stat-Kon DX02437 is a compound based on Polycarbonate resin containing conductive carbon powder, with good impact-resistance, flow and ESD performance, suitable for semi-con industry. |
|||
Flexural Yield Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL FXN121BK PPE+HIPS (Europe-Africa-Middle East) Noryl* FXN121BK is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r.. |
|||
Flexural Yield Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL FXN121LG PPE+HIPS Noryl* FXN121LG is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r.. |
|||
Flexural Yield Strength | 92.0 MPa | 13300 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® FXE1434T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1434T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers extreme low temperature (-40 C) ductility in combination with me.. |