Mechanical Properties Metric English Comments
Flexural Yield Strength 958 MPa
139000 psi
Sheet Stress
Hardwire 3S-23-12 High Density Composite
The 3S Hardwire is a high carbon steel cord with a micro-fine brass or AO-brass (Adhesion Optimized) coating. The 3S cord is used where balanced compressive and tensile strengths are required and re..