Polymer Property : Flexural Yield Strength = 156500 psi
Polymer Property :
Flexural Yield Strength =
156500 psi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Flexural Yield Strength
1079
MPa
156500
psi
Material as cured; RT
Hexcel® HexPly® 922-1/35%/G926 180°C Curing Epoxy Matrix
5H satin/370g/m2 carbon fabric: FVC=60%Information provided by HexCel