Mechanical Properties Metric English Comments
Flexural Yield Strength 53.0 - 168 MPa

@Temperature -40.0 - 80.0 °C
7690 - 24400 psi

@Temperature -40.0 - 176 °F
Average value: 114 MPa Grade Count:1
Overview of materials for Nylon 6, 30% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ..