Polymer Property : Flexural Yield Strength = 1800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 12.4 MPa
1800 psi
13 mm/min; ASTM D790
PolyOne Gravi-Tech™ GRV-UR-045-SS-W Black Polyurethane, Unspecified (PUR, Unspecified)
Information provided by PolyOne
Flexural Yield Strength 12.4 - 33.8 MPa
1800 - 4900 psi
Average value: 26.1 MPa Grade Count:4
Overview of materials for PVC, Foam Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Foam Grade". Each property range of values reported is minimum and maximum values of appropriate Ma..