Mechanical Properties Metric English Comments
Flexural Yield Strength 8.00 - 148 MPa

@Temperature -40.0 - 120 °C
1160 - 21500 psi

@Temperature -40.0 - 248 °F
Average value: 55.1 MPa Grade Count:8
Overview of materials for Nylon 6, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri..