Polymer Property : Flexural Yield Strength = 24200 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 167 MPa
24200 psi
DIN 53455; ASTM D790
Kolon SPESIN® KP212G15VO G/F Reinforced & Retardant PBT Resin  (discontinued **)
SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea..
Flexural Yield Strength 167 MPa

@Thickness 3.20 mm
24200 psi

@Thickness 0.126 in
1.3mm/min; ASTM D790
LG Chemical LUMID GP2130A(W) PA6+GF13%, General Purpose
Feature: Injection Molding, PA6+GF13%, General PurposeApplication: Automotive PartsCAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical
Flexural Yield Strength 167 MPa

@Thickness 3.20 mm
24200 psi

@Thickness 0.126 in
1.3mm/min; ASTM D790
LG Chemical LUMID GP2130B(W) PA66+GF13%, General Purpose
Feature: Injection Molding, PA66+GF13%, General PurposeApplication: Valve CoversCAS No. 32131-17-2, 65997-17-3 and 9010-79-9Information provided by LG Chemical
Flexural Yield Strength 167 MPa

@Thickness 3.20 mm
24200 psi

@Thickness 0.126 in
1.3mm/min; ASTM D790
LG Chemical LUMID HI2202B(W) PA66+GF20%, High Impact
Feature: Injection Molding, PA66+GF20%, High ImpactApplication: Automotive (Covers)CAS No. 25038-54-4, 9010-79-1 and 65997-17-3Information provided by LG Chemical
Flexural Yield Strength 167 MPa

@Thickness 3.20 mm
24200 psi

@Thickness 0.126 in
1.3mm/min; ASTM D790
LG Chemical LUPOY GN2201FM PC+GF20%, Halogen Free, Flame Retardant, Heat Resistance
Description: Injection Molding, PC+GF20%, Halogen Free Flame Retardant, Heat ResistanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information prov..
Flexural Yield Strength 167 MPa
24200 psi
ASTM D790
Samyang Tribit® 1551GN30 PBT, Impact
Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1551GN30 is an impact grade.Information pro..
Flexural Yield Strength 167 MPa
24200 psi
ASTM D790
Samyang Trirex® 3500G20 Polycarbonate, 20% Glass Reinforced
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
Flexural Yield Strength 167 MPa
24200 psi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL GFN2 PPE+PS
PPE+PS blend. 20% Glass reinforced. UL746C F1. NSF 61 listing in several colors (restrictions apply). FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional sta..
Flexural Yield Strength 167 MPa
24200 psi
ASTM D790
Tipco Tipcolene® SEB 400 - 40% Chemically Coupled Glass Fibers Polypropylene Homopolymer with High Heat Stability
40% Chemically Coupled Glass Reinforced PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Flexural Yield Strength 167 MPa
24200 psi
ASTM D790
Cheng Yu Plastic ML3420 PC, 20% Glass Fiber
Flexural Yield Strength 167 MPa
24200 psi
ASTM D790
Cheng Yu Plastic NG1250S Nylon 66, 25% Glass Fiber Reinforced
Flexural Yield Strength 167 MPa
24200 psi
ASTM D790
Cheng Yu Plastic A706G1 SAN, 10% Glass Fiber
Flexural Yield Strength 167 MPa
24200 psi
ASTM D790
PlastxWorld CEVIAN® B2706 30% GF PBT/ABS Alloy
Glass fiber reinforced PBT/ABS alloy.Information provided by PlastxWorld Inc.
Flexural Yield Strength 167 MPa
24200 psi
DIN 53452; ASTM D790
Kolon Kopa® KN173MS Nylon 6 Resin
KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c..