Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Yield Strength = 248 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 248 MPa
36000 psi
ASTM D790
Performance Polymers IPS II PPL-C4219 PEKK (Polyetherketoneketone) Linear Wear Grade
Black pellets; Carbon fiber/PTFE/Graphite compoundInformation provided by Infinite Polymer System II.
Flexural Yield Strength 248 MPa
36000 psi
ASTM D790
Techmer ES Plaslube® J-1/30/SI/2 Nylon 66, 30% GFR, 2% Silicone
Plaslube silicone lubricated nylon 66 grades are cost-effective wear and friction materials with low coefficients of friction. These grades have a potential for noise reduction due to the migratory..
Flexural Yield Strength 248 MPa
36000 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP OF008A PPS (Asia Pacific)
LNP* Thermocomp* OF008A is a compound based on PPS - Branched resin containing Glass Fiber.This product is also known as Thermocomp* OF-1008.
Flexural Yield Strength 248 MPa
36000 psi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL GTX GTX830 PPE+PS+PA
30% Glass Reinforced PPE+PA Alloy.
Flexural Yield Strength 248 MPa
36000 psi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL GTX GTX830 PPE+PS+PA (Asia Pacific)
GR 30%. Highest stiffness of 1200000 psi (8200 MPa) flexural modulus. Excellent chemical and high heat resistance. Application: under the bonnet.
Flexural Yield Strength 248 MPa
36000 psi
ASTM D790
Clariant Renol 60G33HSL Nylon 6, 33% Glass Fiber Reinforced, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
Flexural Yield Strength 248 MPa
36000 psi
ASTM D790
Clariant Renol 60G33-L Nylon 6, 33% Glass Fiber Reinforced, Lubricated
Data provided by Clariant Masterbatches
Flexural Yield Strength 248 MPa
36000 psi
ASTM D790
Clariant Renol PA113G33HR Nylon 66, 33% Glass Fiber, Heat Stabilized, Hydrolysis Resistant
Data provided by Clariant Masterbatches
Flexural Yield Strength 248 MPa
36000 psi
ASTM D790
Clariant Renol PA213G30 Nylon 6, 30% Glass Fiber, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
Flexural Yield Strength 248 MPa
36000 psi
ASTM D790
Clariant Renol PA213G33 Nylon 6, 33% Glass Fiber, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
Flexural Yield Strength 248 MPa
36000 psi
ASTM D790
Clariant Renol PA213G36S Nylon 6, 36% Glass Fiber, Heat Stabilized, Silicone Lubricated
Data provided by Clariant Masterbatches