Polymer Property : Flexural Yield Strength = 28400 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 196 MPa
28400 psi
23°C; 50% RH; ASTM D570
PTS Lucet® GC-225 25% Glass Reinforced Acetal Copolymer
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Flexural Yield Strength 196 MPa
28400 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP DFL38 PC
LNP* Lubricomp* DFL-4038 is a Polycarbonate containing 40% Glass Fiber, 15% PTFE. Added features include: Internally Lubricated.
Flexural Yield Strength 196 MPa

@Thickness 3.20 mm
28400 psi

@Thickness 0.126 in
1.3mm/min; ASTM D790
LG Chemical LUCEL GC225 POM+GF25%, High Rigidity
Feature: Injection Molding, POM+GF25%, High RigidityApplication: Casings of Pump and Pivot BearingsCAS No. 66455-31-0 and 65997-17-3Information provided by LG Chemical
Flexural Yield Strength 196 MPa

@Thickness 3.20 mm
28400 psi

@Thickness 0.126 in
1.3mm/min; ASTM D790
LG Chemical LUMID LW4403A(W) PA66+GF/MF40%, Low Warpage
Feature: Injection Molding, PA66+GF/MF40%, Low WarpageApplication: Automotive (Timing Belt Cover)CAS No. 25038-54-4, 13983-17-0 and 65997-17-3Information provided by LG Chemical
Flexural Yield Strength 196 MPa
28400 psi
DIN 53455; ASTM D790
Kolon KOPA® KN333G15 G/F Reinforced Nylon 66
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin..
Flexural Yield Strength 196 MPa
28400 psi
DIN 53455; ASTM D790
Kolon KOPA® KN135HB30HI Multi Reinforced Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
Flexural Yield Strength 196 MPa
28400 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Valox® IQ507 PBT+PC
Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte..
Flexural Yield Strength 196 MPa
28400 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Valox® IQ507 PBT+PC (Asia Pacific)
Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte..
Flexural Yield Strength 196 MPa
28400 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Valox® IQ507 PBT+PC (Europe-Africa-Middle East)
Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte..
Flexural Yield Strength 196 MPa
28400 psi
ASTM D790
Shinkong Synthetic Fibers Shinite® T101G30 PET, 30% Glass Filled
Information from Shinkong Synthetic Fibers Corp.
Flexural Yield Strength 196 MPa
28400 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP LF004E PEEK (Europe-Africa-Middle East)
LNP* THERMOCOMP* LF004E is a compound based on Polyetheretherketone resin containing Glass Fiber. Added features include: Easy Molding.
Flexural Yield Strength 196 MPa
28400 psi
ASTM D790
Samyang Tribit® 1500G30 Polybutylene Terephthalate, 30% Glass Reinforced
Characteristics:G/F reinforcedHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll infor..
Flexural Yield Strength 196 MPa
28400 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP QF0069 PA6.10 (Europe-Africa-Middle East)
LNP* THERMOCOMP* QF0069 is a compound based on PA610 resin contaning Glass Fiber, Flame Retardant. Added features include: Flame retardant.
Flexural Yield Strength 196 MPa
28400 psi
ASTM D790
Shinkong Synthetic Fibers Shinite® T101G30 PET, 30% Glass Filled
Information from Shinkong Synthetic Fibers Corp.
Flexural Yield Strength 196 MPa
28400 psi
ASTM D790
Shinkong Synthetic Fibers Shinite® E202G30 PBT, 30% Glass Filled
Information from Shinkong Synthetic Fibers Corp.
Flexural Yield Strength 196 MPa
28400 psi
ASTM D790
Shinkong Synthetic Fibers Shinite® E202G30 PBT, 30% Glass Filled
Information from Shinkong Synthetic Fibers Corp.
Flexural Yield Strength 196 MPa
28400 psi
ASTM D790
Toyobo Vylopet® EMC120S Glass Reinforced Polyester, Standard Grade
Key Feature: Flame retardant V-0 UL-94 classApplications: Electric and electronic componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strengt..
Flexural Yield Strength 196 MPa
28400 psi
ASTM D790
Cheng Yu Plastic A707G25 SAN, 25% Glass Fiber
Flexural Yield Strength 196 MPa
28400 psi
DIN 53455; ASTM D790
Kolon KOPA® KN3321G15VO G/F Reinforced & Flame Retardant Nylon 66
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstanding ..
Flexural Yield Strength 196 MPa

@Thickness 3.20 mm
28400 psi

@Thickness 0.126 in
1.3mm/min; ASTM D790
LG Chemical LUMID LW4009A(W) PA6+GF/MF40%, Low Warpage
Feature: Injection Molding, PA6+GF/MF40%, Low WarpageApplication: Automotive (Timing Belt Cover)CAS No. 25038-54-4, 13983-17-0 and 65997-17-3Information provided by LG Chemical