Polymer Property : Flexural Yield Strength = 29890 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 206.1 MPa
29890 psi
ASTM D790
Plenco 50130 PET, Pellet, Injection Molded, Black  (discontinued **)
PLENCO 50130 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in natural and black.Informat..