Mechanical Properties Metric English Comments
Flexural Yield Strength 224 MPa
32500 psi
ASTM D790
Solvay Specialty Polymers Amodel® AFA-6133 V0 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry As Molded &nbs
AMODEL AFA-6133 V0 is a 33% glass-fiber reinforced grade of polyphthalamide (PPA) resin that was developed specifically for connector applications requiring compatibility with both "infrared" and "v..
Flexural Yield Strength 224 MPa
32500 psi
ASTM D790
Techmer ES HiFill® SPS GF40 BK 40% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightFeatures: SyndiotacticAppearance: BlackInformation provided by TP Composites, Inc.